Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADIFLAM A FRX 328 BK - PA66 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADIFLAM A FRX 328 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radiflam A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
PA66 flame retardant injection moulding grade with enhanced mechanical properties retention after thermal aging. Enhanced flowability. Halogen and phosphorus free. Black colour.

Suitable for parts where fire retardancy is required. Rated V-0 at 0.25 mm according to UL-94.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 1.1 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.1 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 3600 / 2450 MPa ISO 527
简支梁缺口冲击强度, +23°C 3 / 5 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 260 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 70 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 200 / * °C ISO 75-1/-2
维卡软化温度, B 220 / * °C ISO 306
线性热膨胀系数, 平行 79 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 90 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 V-0 / * class IEC 60695-11-10
测试用试样的厚度 0.2 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 V-0 / * class IEC 60695-11-10
测试用试样的厚度 0.4 / * mm -
Yellow Card 现存 是的 / * - -
电性能干 / 已调节单位Test Standard
ISO数据
体积电阻率 1E13 / 1E11 Ohm*m IEC 62631-3-1
表面电阻率 * / 1E10 Ohm IEC 62631-3-2
相对漏电起痕指数 600 / - - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 7.5 / * % 类似ISO 62
吸湿性 1.7 / * % 类似ISO 62
密度 1180 / - kg/m³ ISO 1183
典型数据
加工方法
注塑
供货形式
碎粒料, 黑色
添加剂
脱模助剂
特殊性能
阻燃的, 无卤, 无磷, 经热稳处理的/耐热的
地区供应
其他信息
注塑成型
该材料用防水包装运输,已经为后续加工准备好。最合适的加工含水量最大值推荐为0.1%。除湿干燥机的典型条件:温度80°C,露点-20°C或更低,时间2-4h或更多。为了更好加工,避免过大剪切速率和高热应力。注意避免材料吸水以及添加再粉碎材料时混入其他聚合物的污染。颜色变化及机械性能下降可能会发生,需要仔细监控。

Injection Molding 加工参数
熔融温度 模具温度 注塑速
270 - 290°C 60 - 80°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.